Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
TDS MDS
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
DEUREX A 20 K
Bio based Ethylene-Bis-Stearamide wax, fine granules
Drop point °C
142-151
Acid value mg KOH/g
≤ 10
Viscosity 140 °C, mPas
≤ 20
Penetration dmm
1-3
Density (Wax) g/cm³
0,98-1,00
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
105-115
Acid value mg KOH/g
≤ 1
Viscosity 140 °C, mPas
≤ 1
Penetration dmm
2-8
Density (Wax) g/cm³
0,90-0,92
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
90-99
Acid value mg KOH/g
0
Viscosity 140 °C, mPas
≤ 40
Penetration dmm
10-25
Density (Wax) g/cm³
0,94-0,96
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
112-120
Acid value mg KOH/g
0
Viscosity 140 °C, mPas
400-600
Penetration dmm
2-3
Density (Wax) g/cm³
0,93-0,94
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
110-120
Acid value mg KOH/g
0
Viscosity 140 °C, mPas
≤ 40
Penetration dmm
2-5
Density (Wax) g/cm³
0,94-0,96
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
100-110
Acid value mg KOH/g
0
Viscosity 140 °C, mPas
≤ 40
Penetration dmm
10-25
Density (Wax) g/cm³
0,94-0,96
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
110-120
Acid value mg KOH/g
0
Viscosity 140 °C, mPas
≤ 80
Penetration dmm
3-7
Density (Wax) g/cm³
0,94-0,96
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
98-110
Acid value mg KOH/g
0
Viscosity 140 °C, mPas
≤ 200
Penetration dmm
3-4
Density (Wax) g/cm³
0,93-0,94
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
115-123
Acid value mg KOH/g
0
Viscosity 140 °C, mPas
≤ 700
Penetration dmm
≤ 1
Density (Wax) g/cm³
0,93-0,94
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
105-120
Acid value mg KOH/g
0
Viscosity 140 °C, mPas
500-700
Penetration dmm
≤ 2
Density (Wax) g/cm³
0,91-0,96
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
110-120
Acid value mg KOH/g
-
Viscosity 140 °C, mPas
≤ 400
Penetration dmm
≤ 3
Density (Wax) g/cm³
0,93-0,95
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
98-112
Acid value mg KOH/g
≤ 19
Viscosity 140 °C, mPas
≤ 120
Penetration dmm
5-10
Density (Wax) g/cm³
0,96
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
106-114
Acid value mg KOH/g
17
Viscosity 140 °C, mPas
≤ 300
Penetration dmm
2-4
Density (Wax) g/cm³
0,95
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
137-139
Acid value mg KOH/g
6-8
Viscosity 140 °C, mPas
≤ 30000
Penetration dmm
≤ 1
Density (Wax) g/cm³
0,98
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
137-139
Acid value mg KOH/g
15-17
Viscosity 140 °C, mPas
≤ 9000
Penetration dmm
≤ 1
Density (Wax) g/cm³
0,98
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
137-139
Acid value mg KOH/g
24-26
Viscosity 140 °C, mPas
≤ 5000
Penetration dmm
≤ 1
Density (Wax) g/cm³
0,97-0,99
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
137-139
Acid value mg KOH/g
28-32
Viscosity 140 °C, mPas
≤ 4000
Penetration dmm
≤ 1
Density (Wax) g/cm³
0,98
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
137-139
Acid value mg KOH/g
34-36
Viscosity 140 °C, mPas
≤ 3000
Penetration dmm
≤ 1
Density (Wax) g/cm³
0,98
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
100-113
Acid value mg KOH/g
5-9
Viscosity 140 °C, mPas
≤ 20
Penetration dmm
3-6
Density (Wax) g/cm³
0,93
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
100-113
Acid value mg KOH/g
10-14
Viscosity 140 °C, mPas
≤ 20
Penetration dmm
6-10
Density (Wax) g/cm³
0,93
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
100-110
Acid value mg KOH/g
15-19
Viscosity 140 °C, mPas
≤ 20
Penetration dmm
7-11
Density (Wax) g/cm³
0,93
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
100-110
Acid value mg KOH/g
20-24
Viscosity 140 °C, mPas
≤ 20
Penetration dmm
9-12
Density (Wax) g/cm³
0,93
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
96-104
Acid value mg KOH/g
0
Viscosity 140 °C, mPas
200-600
Penetration dmm
6-10
Density (Wax) g/cm³
0,93-0,95
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
110-120
Acid value mg KOH/g
0
Viscosity 140 °C, mPas
≤ 20
Penetration dmm
≤ 2
Density (Wax) g/cm³
0,94-0,95
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
112-120
Acid value mg KOH/g
0
Viscosity 140 °C, mPas
≤ 20
Penetration dmm
≤ 1
Density (Wax) g/cm³
0,94-0,95
Drop point
°C
Acid value
mg KOH/g
Viscosity
140 °C, mPas
Penetration
dmm
Density (Wax)
g/cm³
Drop point °C
142-151
Acid value mg KOH/g
≤ 5
Viscosity 140 °C, mPas
≤ 20
Penetration dmm
1-3
Density (Wax) g/cm³
0,98-1,00